Phosphating (3)
Process is very sensitive to contamination
- do not touch after phosphating
Operating at higher temperature refines grain size (better paint adhesion)
- typically 50oC with agitation
Typical layers contain 0.5 to 1.2% Ni
- environmental concerns (nickel disposal)
- use copper +hydroxylamine accelerator